Sign In | Join Free | My adobecards.com
China Shenzhen Yujies Technology Co., Ltd. logo
Shenzhen Yujies Technology Co., Ltd.
Shenzhen Yujies Technology Co., Ltd.
Verified Supplier

6 Years

Home > PZT Powder >

Navy Type III Hard Material Piezo Powder For Beauty Head Piezo Ceramic

Shenzhen Yujies Technology Co., Ltd.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

Navy Type III Hard Material Piezo Powder For Beauty Head Piezo Ceramic

Brand Name : YUJIE

Model Number : P81

Certification : ISO9001

Place of Origin : Jiangsu, China

MOQ : 1 Kg

Price : Negotiable

Payment Terms : T/T, Western Union

Delivery Time : 3~30 working days

Packaging Details : Carton #: 32x20x18cm

Contact Now

PZT Powder of P-81 Navy Type III Hard Material For Beauty Head Piezo Ceramic

The material performance of piezoelectric ceramic
Num Name of Performance parameter symbol index Allow the public errand
P-33 P-44 P-51 P-81
1 Electromechanical coupling coefficient Kp 0.60 0.60 0.65 0.53 ±6.0%
K31 0.36 0.36 0.38 0.31
K33 0.70 0.70 0.74 0.63
K15 0.70 0.70 0.72 0.66
Kt 0.47 0.48 0.50 0.47
2 The relative electric capacity rate of freedom
ε T

1725 1350 2100 1025 ±12.5%
ε T

1725 1900 2400 1400
3 The medium losses tgδ 0.020 0.005 0.020 0.004
4 The gentle and agreeable constant of elasticity
(x10-12m2/N)
S E
11

15 13 15 11.0 ±10%
S D
33

9.0 8.5 9.0 8.5
S D
55

25 21.5 22.0 21.0
5 Piezoelectricity meet an emergency the constant
(x10-12m/v或C/N)
d31 160 -150 -210 -100 ±12.5%
d33 390 320 450 225
d15 480 530 710 450
6 Mechanical cue Qm 75 400 70 800
7 Frequency constant
(Hz•m)
Nd 1950 2200 2000 2300 ±5%
N1 1470 1600 1450 1700
N3 1880 2000 1900 1960
N5 1130 1230 1200 1230
Nt 2250 2300 2250 2280
8 The velocity of sound
(m/s)
Vd 3000 3300 3000 3500 ±5%
V1 2940 3200 2900 3400
V3 3760 4000 3800 3920
V5 2260 2460 2400 2460
Vt 4500 4600 4500 4560
9 Density (x103kg/m3) ρ 7.6 7.5 7.45 7.45
10 Curie's temperature () Tc 335 300 260 300
11 Rate of change of time of ten times
(%)
ANd 0.20 1.2 0.35 1.3
AKp -0.25 -1.8 -0.4 -2.0
-1.5 -4.0 -1.5 -4.0
12 The relative rate of change of temperature (%)-10℃~50℃ The datum 25℃ ΔNd/N 1.0 1.0 1.5 1.5
Δε/ε 15 9.0 20 9.0
13 The strong field lies between electric performance
T=25℃ E=400V
tgδ 0.04 0.01
Δε/ε 0.17 0.06
note: 1, Index besides Curie's temperature, is the measurement value for ten days after polarizing for the performance parameter index in the form .

Product Tags:

piezo powder

      

piezoceramic materials

      
 Navy Type III Hard Material Piezo Powder For Beauty Head Piezo Ceramic Manufactures

Navy Type III Hard Material Piezo Powder For Beauty Head Piezo Ceramic Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Shenzhen Yujies Technology Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)